Can any one point me in a good direction?
Also what is the "best" Silicone to use?
Thanks,
Matt
Scratchbuilders!: Armor/AFV
This is a group for armor scratchbuilding questions, topics and projects.
This is a group for armor scratchbuilding questions, topics and projects.
Hosted by Mike Kirchoff
Resin Casting "Starter Set"
matt
Campaigns Administrator
New York, United States
Member Since: February 28, 2002
entire network: 5,957 Posts
KitMaker Network: 2,626 Posts
Member Since: February 28, 2002
entire network: 5,957 Posts
KitMaker Network: 2,626 Posts
Posted: Sunday, August 11, 2002 - 09:55 PM UTC
ekaufman
Haifa, Israel
Member Since: June 17, 2002
entire network: 217 Posts
KitMaker Network: 0 Posts
Member Since: June 17, 2002
entire network: 217 Posts
KitMaker Network: 0 Posts
Posted: Sunday, August 11, 2002 - 10:01 PM UTC
You can try smooth-on strater kit, you get RTV,Resin,Sealer and release agent.
plus their informative booklet. all for about 25 USD.
http://www.smooth-on.com
plus their informative booklet. all for about 25 USD.
http://www.smooth-on.com
sgtreef
Oklahoma, United States
Member Since: March 01, 2002
entire network: 6,043 Posts
KitMaker Network: 1,603 Posts
Member Since: March 01, 2002
entire network: 6,043 Posts
KitMaker Network: 1,603 Posts
Posted: Sunday, August 11, 2002 - 11:59 PM UTC
Here is another one you might want to look at.
http://www.alumilite.com/ amd one more
http://www.dowcorning.com/FAQ/faq_search.asp?DCWS=Moldmaking&DCWSS=&ind=013&2ndlevel=
I have been using Dow for about 15 years and have molds that are 10 years old while I have not casted anything in about 7 years,these molds are still good and usable
http://www.alumilite.com/ amd one more
http://www.dowcorning.com/FAQ/faq_search.asp?DCWS=Moldmaking&DCWSS=&ind=013&2ndlevel=
I have been using Dow for about 15 years and have molds that are 10 years old while I have not casted anything in about 7 years,these molds are still good and usable